Plastic Board Extrusion Mould Manufacturer

Plastic board extrusion moulds are the core components of plastic extrusion production lines, determining the final cross-sectional shape, dimensional accuracy, surface quality, and production stability of the board.
Essentially, it is a precision device that takes high-temperature molten plastic from the extruder, passes it through a specific flow channel structure to form a uniform, constant-speed, and constant-pressure flat rectangular melt flow, and finally cools and solidifies it into a sheet of the required specifications.
Anhui Weilei board extrusion Dies adhere to precision manufacturing and innovative design, committed to providing customers with high-quality board materials characterized by stable flow lines, uniform thickness, and low internal stress.
Utilizing advanced computer flow channel simulation and precision machining processes, each die set ensures excellent output stability, outstanding self-cleaning properties, and broad material adaptability, making it the ideal choice for enhancing product competitiveness and achieving efficient and stable production.

Extrusion Mould Production Process

Flooring-1 Flooring-1
Weilei Mould

Types of Plastic Board Extrusion Moulds

Weilei board extrusion molds cover PVC foam board without choke bar single-runner, dual-channel, co-extrusion, acrylic molds, etc. We are committed to providing customers with high-quality board extrusion molds through precise and reliable solutions.

PVC Foam Board Dual-Runner Mould

PVC Foam Board Dual-Runner Mould

Applicable Products Thickness Range: 25-40mm
Main Application: Entire door panel, furniture board, building templates, etc.

Read More
PVC Foam Board Mould,Calibrator

PVC Foam Board Mould,Calibrator

Applicable products thickness range: 5-25mm
Main Application: Poster board, decoration board, monobloc door panel, furniture board, building templates, etc.

Read More
PVC Foam Board without Choke bar Single-Runner Mould

PVC Foam Board without Choke bar Single-Runner Mould

Applicable products thickness range: 5-25mm
Main Application: Cabinets board, furniture board, decoration board, floor board, building board, bricks trays,etc.

Read More
PVC Foam Board Co-extrusion Mould、Co-extrusion Distributor

PVC Foam Board Co-extrusion Mould、Co-extrusion Distributor

Applicable products thickness range: 5-25mm
Main Application: Cabinets board, furniture board, decoration board, building templates, floor boards, brick trays, poster boards, etc.

Read More
PMMA Acrylic Mold

PMMA Acrylic Mold

Applicable products thickness range: 0.5-10mm
Main Application: Light boxes, lamps, electronic instruments, decorative composite materials, etc.

Read More
PP/PC/PS Mould

PP/PC/PS Mould

Applicable products thickness range: 3-40mm
Main Application: Composite materials, food packaging, etc.

Read More
Weilei Mould

Production of Different Plastic Boards

Plastic board extrusion molds produce a wide variety of plastic boards, mainly including PVC, PP, PS, PC, PMMA board, etc. These boards meet the diverse needs of various industries due to their advantages of dimensional stability, smooth surface, and continuous and efficient production.

PVC Foam Board
PVC Foam Board
PVC Foam Board
PVC Foam Board
PMMA Board
PVC Foam Board
Acrylic Board
HIPS Board
Weilei Mould

Plastic Board Extrusion Main Application

Weilei Mould

OUR ADVANTAGE

Frequently Asked Question

  • What to do if the board is thicker in the middle and thinner at the edges?
    Thicker in the middle and thinner at the edges: This indicates that the material is exiting too quickly in the middle. Slightly tighten the flow-restricting bolts in the middle area of ​​the mold and/or slightly lower the die lip clearance in the middle area to increase resistance in the middle section.
    * Important principle: "Fine-tuning" - Each adjustment should be small (such as 1/8 or 1/4 of a turn), and wait for a period of time to stabilize (such as 10-30 minutes) before observing the effect. Avoid making large adjustments.
  • Are there lines or scratches on the surface of the board?
    It's highly likely that the mold lip is damaged or dirty. The machine needs to be stopped, and the mold lip exit point should be carefully cleaned and polished using a copper or soft scraper.
  • How to clean when changing materials or colors?
    Use new material or a special cleaning agent to eject the old material. Clean the die opening immediately after stopping the machine with a soft tool. Never use hard steel objects to scrape it.
  • How should molds be maintained on a daily basis?
    * Start-up: Slowly heat up for even heating.
    * Production: Clean using only soft tools (copper, wood).
    * Shutdown: For long-term storage, rinse thoroughly with cleaning agent, apply rust-preventive oil, and slightly open the mold lip before storage.
  • Unstable material ejection at the mold edge, with flash?
    Inspect and tighten the end caps (end plates) at both ends of the mold. You can try slightly reducing the temperature at both ends of the mold or tightening the end lip.