Plastic Sheet Extrusion Mould Manufacturer

Sheet Extrusion Dies are primarily composed of key components such as the die body, lip, adjustment mechanism, connection flange, and heating temperature control system. Through precise coordination, these parts form a stable forming channel capable of extruding plastic sheets with specific widths and thicknesses.
They are widely used in producing plastic sheets made of PP, PS, PET, ABS, and other materials. These sheets are subsequently utilized in manufacturing various products, including food packaging (such as cups, bowls, and trays), medical device trays, substrates for advertising printing, lining panels for home appliance shells, stationery, and architectural decoration materials.

Extrusion Mould Production Process

Flooring-1 Flooring-1
Weilei Mould

Production of Different PET/PP/PC/PS Sheets

Flooring-1
Flooring-2
Flooring-3
Flooring-4
Weilei Mould

Types of Plastic Sheet Extrusion Moulds

Rigid PVC Laminate Mould

Rigid PVC Laminate Mould

Applicable Products Thickness Range: 0.7-1.5mm
Main Application: Packing tape, Edge band and surface sticking.

Read More
PET Mould

PET Mould

Applicable products thickness range: 0.15-2mm
Main Application: Food packaging, hardware tool packaging,etc

Read More
PP/PC/PS Mould

PP/PC/PS Mould

Applicable products thickness range: 0.15-3mm
Main Application: Composite materials,food packaging,etc.

Read More
Weilei Mould

OUR ADVANTAGE

Frequently Asked Question

  • What should I do if the product surface at the mold exit is not smooth or has scratches?
    This is usually caused by residue or damage inside the die lip (sizing sleeve). Immediately stop the machine, clean the die lip, and check for scratches or rust. Polish if necessary.
  • Why are the dimensions of the extruded products inconsistent, sometimes large and sometimes small?
    There are three main reasons: ① Excessive temperature fluctuations require checking the temperature control system; ② Unstable extruder screw speed or traction speed; ③ Blockage in the internal flow channels or die lip of the die, resulting in uneven material output.
  • Why does the product discharge quickly from the middle but slowly from the sides?
    This is a typical case of "uneven material flow from the die lip". It is necessary to adjust the flow resistance in different areas by adjusting the flow block or bolt in the middle of the die lip to make the material flow rate uniform.
  • What should I do if production of the new mold is not going smoothly from the very beginning?
    New molds require a "break-in period." First, confirm that the mold design parameters match the current materials and equipment. Then, slowly increase the temperature for low-speed preheating and initial adjustments; do not proceed directly to high-speed production.
  • How should molds be cleaned and maintained after daily use?
    Immediately after shutdown, use a pure copper scraper, soft cloth, and special mold cleaner to remove any remaining material. Do not use hard objects such as steel to scrape. After cleaning, apply rust-preventive oil, close the mold, and store.